Nickel and High Temperature Alloys

Alloy Name Trade Name UNS No. British Specs American Specs German Specs French Specs
Alloy 200 Nickel 200 UNS N02200 BS 3072
BS 3073
BS 3074
BS 3075
BS 3076
NA12
ASTM B162
ASTM B163
ASTM B725
ASTM B730
WS 2.4060
WS 2.4066
Alloy 201 Nickel 201 UNS N02201 BS 3072
BS 3073
BS 3074
BS 3075
BS 3076
NA11
ASTM B162
ASTM B163
ASTM B725
ASTM B730
AMS 5553 Sheet and Strip
WS 2.4061
WS 2.4068
Alloy 400 Monel 400 UNS N04400 BS 3072
BS 3073
BS 3074
BS 3075
BS 3076
NA11
AMS 4574 Tube
AMS 4575 (Tube *)

AMS 4675 Bar and Forgings
AMS 4730 Wire
AMS 4731 Wire and Ribbon
AMS 4544 Sheet, Strip and Plate
QQ-N-281
ASTM B164
Alloy 405 Monel 405 UNS N04405 AMS 4674J Bar and Forgings
AMS 7234
QQ-N-281
MIL-N-894
Alloy K500 Monel K500 UNS N05500 BS 3072
BS 3073
BS 3074
BS 3075
BS 3076
NA18
AMS 4676 Bar and Forgings
QQ-N-286
WS 2.4375
Alloy 600 Inconel 600 UNS N06600 BS 3072
BS 3073
BS 3074
BS 3075
BS 3076
NA14
AMS 5580 (Tube *)
AMS 5540 Sheet, Strip and Plate
AMS 5665 Bar and Forgings
AMS 5687 Wire
QQ-W-390
WS 2.4816 AFNOR NC15Fe
Alloy 601 Inconel 601 UNS N06601 AMS 5715 Bar and Forgings
AMS 5870 Sheet, Strip and Plate
ASTM B166
ASTM B167
ASTM B168
ASTM B751
ASTM B775
ASTM B829
WS 2.4851
Alloy 617 Inconel 617 UNS N06617 AMS 5887 Bar and Forgings
AMS 5888 Plate
AMS 5889 Sheet and Strip
WS 2.4663a
Alloy 625 Inconel 625 UNS N06625 BS 3072
BS 3073
BS 3074
BS 3075
BS 3076
NA21
AMS 5581 Tube
AMS 5599 Sheet, Strip and Plate
AMS 5666 Bar, Forgings
AMS 5869 Sheet, Strip and Plate
AMS 5879 Sheet, Strip and Foil
AMS 5837 Welding Wire
WS 2.4856 AFNOR NC22DNb
Alloy 706 Inconel 706 UNS N09706 AMS 5701 Bar and Forgings
AMS 5702 Bar and Forgings
AMS 5703 Bar and Forgings
AMS 5605 Sheet, Strip and Plate
AMS 5606 Sheet, Strip and Plate
Alloy 718 Inconel 718 UNS N07718 AMS 5662 Bar and Forgings
AMS 5663 Bar and Forgings
AMS 5664 Bar and Forgings
AMS 5589 Seamless Tube
AMS 5590 (Tube *)
AMS 5596 Sheet, Strip and Plate
AMS 5597 Sheet, Strip and Plate
AMS 5832 Welding Wire
AMS 5914 Sheet, Strip and Foil
AMS 5950 (718SPF) Sheet & Strip
WS 2.4668
Alloy 722 Inconel 722 UNS N07722 AMS 5541 Sheet and Strip
AMS 5714 Bar and Forgings
Alloy 725 Inconel 725 UNS N07725 ASTM B805
Alloy X750 Inconel X750 UNS N07750
UNS N07752
AMS 5542 Sheet, Strip and Plate
AMS 5582 Seamless Tube
AMS 5583 Seamless Tube
AMS 5747 Bar and Forgings
AMS 5779 Welding Electrodes
AMS 5598 Sheet, Strip and Plate
AMS 5667 Bar and Forgings
AMS 5668 Bar and Forgings
AMS 5669 Bar
AMS 5670 Bar and Forgings
AMS 5671 Bar and Forgings
AMS 5698 Wire
AMS 5699 Wire
WS 2.4669
Alloy X Inconel HX
Hastelloy X
UNS N06002 AMS 5536 Sheet, Strip and Plate
AMS 5754 Bar and Forgings
AMS 5798 Welding Wire
AMS 5587 Seamless Tube
AMS 5588 Welded Tube
Alloy W Hastelloy W UNS N10004 AMS 5755 Bar and Forgings
AMS 5786 Welding Wire
Alloy 800
Alloy 800H
Alloy 800HT
(Welding)
Incoloy 800
Incoloy 800H
Incoloy 800HT
N08800
N08810
N08811
BS 3072
BS 3073
BS 3074
BS 3075
BS 3076
NA15
AMS 5766 Bar and Forgings
AMS 5871 Sheet, Strip and Plate
ASTM B408
ASTM B564
ASTM A240
ASTM A480
WS 1.4876
WS 1.4958
WS 1.4959
Alloy 825 Incoloy 825 UNS N08825 BS 3072
BS 3073
BS 3074
BS 3075
BS 3076
NA16
ASTM B425
ASTM B424
ASTM B163 (Tube *)
WS 2.4858
Alloy 901 Nimonic 901
Incoloy 901
UNS N09901 AMS 5830 Welding Wire
AMS 5660 Bar and Forgings
AMS 5661 Bar and Forgings
WS 2.4662
Alloy 907 Incoloy 907 UNS N19907
Alloy 909 Incoloy 909 UNS N19909 AMS 5884 Bars, Forgings, Rings
AMS 5892 Sheet, Strip
AMS 5893 Bars, Forgings, Rings
Alloy 925 Incoloy 925 UNS N09925
Alloy C276 Inconel C276
Hastelloy C276
UNS N10276 AMS 5750
ASTM B462
ASTM B564
ASTM B574
ASTM B575
ASTM B622
ASTM B626 (Tube *)
ASTM B619
ASTM B775
WS 2.4819
Alloy 75 Nimonic 75
Haynes 75
UNS N06075 BS HR5 Alloy 75 Bar
BS HR203 Alloy 75 sheet
BS HR403 Alloy 75 tube*
BS HR504 Alloy 75 Bar (rivet)
WS 2.4630
WS 2.4951
AFNOR NC 20T
Alloy 80A Nimonic 80A UNS N07080 BS 3072 NA20
BS HR1 Alloy 80A Bar
BS HR201 Alloy 80A sheet
BS HR401 Alloy 80A Tube
BS HR601 Alloy 80A Bar (rivet)
ASTM B637 WS 2.4631
WS 2.4952
AFNOR NC 20TA
Alloy 86 Nimonic 86
Alloy 90 Nimonic 90 UNS N07090 BS HR2 Alloy 90 bar
BS HR202 Alloy 90 sheet
BS HR402 Alloy 90 tube
BS HR501 Alloy 90 wire (springs)
BS HR501 Alloy 90 wire (springs)
AMS 5829 Welding Wire WS 2.4632
Alloy 263 Nimonic 263
Haynes 263
UNS N07263 BS HR10
BS HR206
BS HR404
AMS 5872 Sheet Strip and Plate
AMS 5886 Bar and Forgings
WS 2.4650
Alloy 105 Nimonic 105 BS HR3 WS 2.4634 AFNOR NCKD 20ATv
Alloy 115 Nimonic 115 BS HR4 WS 2.4636 AFNOR NCK 15ATD
Alloy PE11 Nimonic PE11 WS 2.4662 AFNOR Z8 NC D38
Alloy PE16 Nimonic PE16 BS HR55
BS HR207
AFNOR NW 11AC
Alloy PK33 Nimonic PK33 DTD 5057 AFNOR NC19 KDu/v
Waspaloy Waspaloy UNS N07001 AMS 5544 Sheet, Strip and Plate
AMS 5586 Welded Tube
AMS 5828 Welding Wire
AMS 5704 Bar and Forgings
AMS 5706 Bar and Forgings
AMS 5707 Bar and Forgings
AMS 5708 Bar and Forgings
AMS 5709 Bar and Forgings
WS 2.4654
Alloy R41 Rene 41
Udimet alloy R41
UNS N07041 AMS 5545 Sheet, Strip and Plate
AMS 5712 Bars and Forgings
AMS 5713 Bars and Forgings
AMS 5800 Welding Wire
Multimet N155 Multimet UNS R30155 AMS 5532 Sheet, Plate and Strip
AMS 5769 Bars, Rings and Forgings
AMS 5794 Welding Wire
AMS 5795 Coated Electrodes
Alloy 22 Hastelloy C-22 UNS N06022 WS 2.4602
Alloy B-3
Alloy C-4
Alloy B-2 Hastelloy B-2 ASTM B333
Alloy N Hastelloy N UNS N10003 AMS 5771 Bar and Forging
AMS 5607 Sheet, Strip and Plate
Alloy S Hastelloy S UNS N06635 AMS 5711 Bar and Forging
AMS 5838 Welding Wire
AMS 5873 Sheet, Strip and Plate
Alloy 401 Monel 401
Alloy 404 Monel 404
Alloy 450 Monel 450
Alloy 700 Inconel 700
Alloy 702 Inconel 702 UNS N07702 AMS 5550 Sheet, Strip and Plate
Alloy 713C Inconel 713C
Alloy 801 Incoloy 801 UNS N08801 AMS 5552 Sheet, Strip and Plate
Alloy 903 Incoloy 903
Alloy G
Alloy G-35
Alloy G-30
Alloy G-3