Go to - Nickel-Based SuperAlloys - Cobalt-Based SuperAlloys - Low Expansion Nickel-Iron Alloys - Copper Nickel Alloys - Soft Magnetic Alloys - Permanent Magnet Alloys - Titanium Alloy - Stainless Steel
|
||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
| Alloy Name | Trade Name | UNS No. | British Specs | American Specs | German Specs | French Specs |
| Alloy 25 / L605 | Haynes 25 Udimet L605 |
UNS R30605 UNS W73605 |
AMS 5537 Sheet AMS 5759 Bar & Rod AMS 5796 Welding wire AMS 5797 Covered welding rod |
|||
| Alloy 188 | Haynes 188 Udimet 188 |
UNS R30188 | AMS 5608 Sheet, Strip and Plate AMS 5801 Welding Wire |
|||
| MP159 | MP159 | UNS R30159 |
AMS 5842H Bar
AMS 5845 Bar |
|||
| MP35N | MP35N | UNS R30035 | ||||
| Cobalt Alloy 6b | UNS R30016 | AMS 5894 Bar, Sheet, Plate | ||||
| CoCrMo Alloy | ASTM F75 | |||||
| Alloy 1 | UNS R30001 | |||||
| Alloy 6 | UNS R30006 | |||||
| Alloy 12 | UNS R30012 | |||||
| Alloy 21 | UNS R30021 | |||||
| Go to - Nickel-Based SuperAlloys - Cobalt-Based SuperAlloys - Low Expansion Nickel-Iron Alloys - Copper Nickel Alloys - Soft Magnetic Alloys - Permanent Magnet Alloys - Titanium Alloy - Stainless Steel Or use Ctrl F. |
||||||
All Products(40)
- 1
- 2
- 3
- 4
- 5