+86-17335753350

Model No: Rene 62

Rene 62 Nickel-Based Superalloy

Rene 62 is a vacuum-melted nickel-base superalloy offering 1,462 MPa tensile strength, 813°C service temperature, and excellent weldability. Superior to Alloy 718 and Rene 41 below 730°C. Ideal for turbine discs, casings, welded structures, and hot-work tooling. ZYTC Alloy is AS9120B and ISO 9001 certified.
Quantity :
Contact Now
ZYTC Alloy, a professional and reliable Chinese nickel-based superalloy manufacturer and supplier, provides high-quality Rene 62 wrought precipitation-hardening nickel-based superalloy in diversified forms including bar, plate and forging.
 
Produced via strict vacuum smelting processes, Rene 62 features excellent high-temperature oxidation resistance, outstanding weldability and superior high-temperature plasticity. Characterized by a slow age-hardening reaction, this alloy avoids excessive hardening brittleness during service and exhibits extremely stable comprehensive performance.
 
Rene 62 is widely recognized as an ideal material for high-stress welded structural parts, high-temperature thermal forming dies and a variety of aero-engine high-temperature components.

Superior Temperature Resistance & Mechanical Performance Advantages

Rene 62 boasts an extreme maximum service temperature of up to 813°C. When operated continuously at temperatures below 730°C, its tensile strength and yield strength are significantly superior to mainstream superalloys such as Inconel 718 and Rene 41, delivering more reliable load-bearing performance and longer service life under long-term high-temperature and high-load working conditions. Featuring a slow age-hardening reaction and excellent high-temperature plasticity, the alloy effectively avoids brittleness issues and performs exceptionally well in high-stress welded structures and hot forming applications.
 
The alloy maintains balanced strength and ductility at both room temperature and elevated temperatures, with stable and standardized mechanical parameters as shown below:

Chemical composition(mass fraction)(wt.%) of the Rene 62

ElementComposition (wt.%)
C0.02–0.08 (≤)
Si≤ 0.25
Mn≤ 0.25
P≤ —
S≤ —
Cr13.5–16.5
NiBalance (…)
Mo8.5–9.5
Al1.1–1.4
Cu—
Nb2.1–2.5
Ti2.35–2.63
V—
Fe21–24
N—
Co—
Pb—
B—
Other—

Mechanical Properties of steel grade Rene 62

PropertyValue
Yield Strength Rp₀.₂ (MPa)372 (≥)
Tensile Strength Rm (MPa)138 (≥)
Impact KV/Ku (J)33
Elongation A (%)12
Reduction in Cross Section on Fracture Z (%)34
As-Heat-Treated ConditionSolution and Aging, Annealing, Ausaging, Q+T, etc.
Brinell Hardness (HBW)333

Physical Properties of steel grade Rene 62

Temperature (°C)Modulus of Elasticity (GPa)Mean Coeff. of Thermal Expansion (10⁻⁶/°C, between 20°C and)Thermal Conductivity (W/m·°C)Specific Thermal Capacity (J/kg·°C)Specific Electrical Resistivity (Ω·mm²/m)Density (kg/dm³)Poisson's Coefficient ν
11––––0.11––
565598–34.3432–––
922–3311.2––422144

Core Material Characteristics

  • Vacuum Smelting Purity: Adopts professional vacuum smelting process with uniform microstructure, low impurity content and stable batch performance
  • Excellent Weldability & Oxidation Resistance: Good high-temperature oxidation resistance, suitable for complex high-temperature welded structural components without easy cracking or failure
  • Slow Age Hardening Speed: Avoids rapid hardening embrittlement, ensuring stable mechanical performance during long-term high-temperature service
  • Superior High-Temperature Plasticity: Excellent thermal processing performance, easy for hot forging, forming and precision processing
  • Outstanding High-Temperature Strength: Stronger tensile and yield strength than Alloy 718 and Rene 41 below 730°C, perfect for high-stress extreme working conditions

Industrial Applications

Benefiting from its unique high-temperature resistance, high strength, stable aging performance and excellent weldability, Rene 62 superalloy is widely applied in core high-temperature and high-load industrial and aerospace fields:
  • Aero-engine core components: turbine casings, turbine discs, turbine blades, torque rings and various engine structural parts
  • High-temperature welded structural components for aerospace and power equipment
  • High-precision high-temperature thermal forming dies and industrial high-temperature resistant molds
  • High-stress structural parts requiring long-term stable operation under medium and high temperature conditions

Why Choose ZYTC Alloy Rene 62 Superalloy

As a professional Chinese manufacturer of aerospace-grade nickel-based superalloys, ZYTC Alloy strictly produces Rene 62 alloy bar, plate and forging through professional vacuum smelting technology to ensure ultra-low impurity content and uniform microstructure. We implement full-process quality control covering solution treatment, aging hardening and precision finishing, stabilizing the alloy’s unique advantages of slow aging response, excellent weldability and high-temperature ductility. All Rene 62 products are supplied with complete MTR certificates and support third-party testing. We provide standard stock of Rene 62 bars, plates and custom forgings to meet diverse high-end industrial and aerospace project requirements worldwide.
 
Contact ZYTC Alloy now to get free Rene 62 technical datasheets for bar, plate and forging products, detailed parameter reports and competitive factory quotations!
📧 Email: daisy@zytcsteel.com
📲 WhatsApp: +86 17335753350
 
Tianjin ZYTC Alloy Technology Co., Ltd
 
 ZYTC Alloy CERTIFICATION
Inspection Equipment