I. Product Information - Material Name: Inconel 740H Nickel-Chromium-Cobalt Superalloy (UNS N07740 / W.Nr. 2.4663)
- Material Definition: A precipitation-hardenable Ni-Cr-Co superalloy strengthened by gamma-prime (γ′) phase, developed specifically for advanced ultra-supercritical (A-USC) steam service at 700–800 °C.
- Core Value Proposition: The only nickel alloy code-qualified for A-USC boiler construction under ASME Code Case 2702, with a maximum use temperature of 800 °C (1472 °F) and 100,000-hour creep-rupture strength at 750 °C / 35 MPa.
- Key Advantages: Gamma-prime (γ′) strengthening | Excellent creep-rupture strength to 800 °C | Superior coal-ash and steam oxidation resistance | Good weldability with controlled PWHT | ASME Code Case 2702 approved
- Certification:ISO 9001 and AS 9120B certified; full batch traceability; in-house laboratory verification.
- Product Forms: Bar & Rod | Forgings & Rings | Seamless Pipe & Tube | Plate | Welding Wire
If you need a size, temper, heat-treatment condition or certification that is not listed below, send us the drawing — we will confirm mill capability and lead time within one working day. II. Material Standards & Specifications Standard / Specification | Product Form | Description | UNS N07740 | – | Unified numbering system | ASTM B983 / ASME SB983 | Bar, forgings, seamless tube | Precipitation-hardened Ni-Cr-Co alloy – current edition | ASME Code Case 2702 | Sheet, plate, rod, seamless pipe & tube, fittings, forgings | A-USC boiler construction, Section I & B31.1 – max 800 °C | AWS A5.14 ERNiCrCoMo-1 | Welding filler | Matching filler metal for 740H | EN 10204 3.1 | Mill certificate | 3.2 / third-party inspection available on request |
Material must be supplied in the solution heat-treated and aged condition. ASME Code Case status and revisions should be confirmed with ASME before specification. III. Chemical Composition (wt%) Element | Min | Max | Nickel (Ni) | Balance | – | Chromium (Cr) | 23.5 | 25.5 | Cobalt (Co) | 15.0 | 22.0 | Niobium (Nb) | 0.50 | 2.50 | Titanium (Ti) | 1.15 | 1.65 | Aluminum (Al) | 1.20 | 1.75 | Molybdenum (Mo) | 0.30 | 2.00 | Carbon (C) | 0.02 | 0.08 | Manganese (Mn) | – | 0.50 | Silicon (Si) | – | 1.00 | Phosphorus (P) | – | 0.030 | Sulfur (S) | – | 0.015 |
IV. Service Conditions & Material Selection Boundaries Suitable Conditions - Advanced ultra-supercritical (A-USC) superheater and reheater tubing at 700–800 °C
- Thick-section steam headers and main steam piping above 700 °C
- Pressure-containing components exposed to coal-ash corrosion and high-temperature steam oxidation
- Concentrated solar power receivers and high-temperature salt-loop tubing
Typical Applications - Power Generation: A-USC boiler tubes, steam headers, main steam piping, turbine components
- Oil & Gas / Petrochemical: High-temperature pressure piping and heat exchangers
- Concentrated Solar: Receiver and molten-salt loop components
Selection Boundaries - Below 700 °C / cost-sensitive service: consider Inconel 617 or Alloy 800H
- Severe aqueous corrosion: consider Inconel 625 or Hastelloy C-276
- Maximum strength at moderate temperature: consider Inconel 718
V. Manufacturing Process & Heat Treatment Process | Parameters | Outcome | Solution Anneal | ≥ 1100 °C (2010 °F), 1 hr per 25 mm thickness (min 0.5 hr), rapid cool | Dissolves γ′, recrystallizes | Aging | 760–815 °C (1400–1500 °F), min 4 hr up to 50 mm thickness | γ′ precipitation, peak strength | Post-Weld Heat Treatment | 760–815 °C (1400–1500 °F), mandatory per Code Case 2702 | Restores properties in weld zone |
Fabrication: Welding by GTAW / SAW with matching ERNiCrCoMo-1 filler; PWHT is mandatory; a weld strength reduction factor of 0.70 applies above 600 °C for longitudinal seams. Hot working at 1050–1150 °C. Cold forming above 5 % strain requires full solution + aging re-treatment of the entire component. Machining with rigid setups, positive feeds and sharp carbide tooling. VI. Mechanical Properties Condition: Solution Treated + Aged (Room Temperature) Property | Typical / Minimum Value | Tensile Strength | ≥ 1000 MPa (145 ksi) | Yield Strength (0.2 % offset) | ≥ 620 MPa (90 ksi) | Elongation | ≥ 20 % | Hardness | Contact for certified test reports |
Elevated-Temperature Tensile (transverse, aged): Temperature | Yield Strength | Tensile Strength | 700 °C (1292 °F) | 567 MPa (82.2 ksi) | 861 MPa (124.9 ksi) | 750 °C (1382 °F) | 596 MPa (86.4 ksi) | 818 MPa (118.6 ksi) | 800 °C (1472 °F) | 594 MPa (86.2 ksi) | 691 MPa (100.2 ksi) |
Design stress values (Su, Sy) per ASME Code Case 2702 Tables 5/5M and 6/6M. Certified test reports available on request. VII. Material Comparison Guide Dimension | Alloy 740H | Alloy 617 | Alloy 625 | Alloy 718 | Primary Strength | Creep strength to 800 °C | Solid-solution strength | Corrosion + strength | Highest strength to 704 °C | Strengthening | Gamma-prime (γ′) | Solid-solution | Solid-solution | Gamma-double-prime (γ″) | Max Use Temperature | 800 °C (code-approved) | ~980 °C | ~980 °C | ~704 °C | Coal-Ash Corrosion | Excellent | Good | Moderate | Poor | Weldability | Good (with PWHT) | Excellent | Excellent | Excellent | Typical Use | A-USC boilers, steam piping | Gas turbines, chemical | Marine, chemical, FGD | Aerospace, oil & gas tools |
  
Procurement Recommendation: ChooseInconel 740H for A-USC boiler and steam piping where code-approved creep strength and coal-ash corrosion resistance above 700 °C are required. Choose Alloy 617 for lower-cost high-temperature service without code qualification. Choose Alloy 625 for severe aqueous corrosion. Choose Alloy 718 for maximum room/moderate-temperature strength and easier fabrication. Request a Quote or Sample Today For A-USC power generation and high-temperature pressure applications demanding Inconel 740H performance, contact ZYTC Alloy today. Our technical team is ready to assist with material selection, heat treatment specification and code compliance. Contact Us: Email: daisy@zytcsteel.com | WhatsApp / WeChat: +86 17335753350 |